WeChat QR code

Advanced EVA POE Foam Solution

IUS-4065
Ultra-Soft, Low-Shrink Elastomer

Ultra-soft TPE for EVA/POE foam, combining Shore A 40 hardness and an approximately 64°C melting point to support dimensional stability during secondary processing.

Shore 40 AHardness
≈ 64°CMelting Point
ExcellentHeat shrinkability
ExcellentDimension stability
ExcellentProcess Stability
Request a sample to validate your formulation and processing conditions
阅读统计: 模块内容不存在
R&D Challenge

Why Ultra-Soft Midsoles Are Prone to Secondary Shrinkage

Low-hardness POE improves softness and feel, but secondary heating can relax the foam structure and cause edge shrinkage, warping, dimensional deviation and lamination misalignment. The real development challenge is to reduce hardness while maintaining rebound and controlling dimensional change after heating and lamination.

Softness

Lower finished-product hardness for improved cushioning, conformity and underfoot comfort.

Processing Stability

Reduce secondary dimensional change after baking, hot pressing and lamination.

Production Yield

Reduce left-right variation, lamination misalignment and batch-to-batch appearance variation.

Material Selection Trade-off

The Material-Selection Trade-Off: Softer Materials Can Shrink More Under Heat

To achieve exceptional softness and high rebound, midsole formulations often use TAFMER™ or ENGAGE™ POE. TAFMER™ DF640 and ENGAGE™ 8842 typically measure Shore A 54–56 and offer excellent softness and feel, but their melting transition is below 50°C. Lamination, baking or hot pressing above this range can relax the foam structure and increase the risk of secondary shrinkage, edge contraction and warping.

MaterialRaw-material hardnessDSC melting peakPrimary advantageFormulation and processing considerations
TAFMER™ DF640Approx. 54–56ABelow 50°CGood softness and feelDimensional stability after reheating must be validated
ENGAGE™ 8842Approx. 54–56ABelow 50°CGood softness and elasticityThermal shrinkage may occur after lamination and baking
IUS-4065Approx. 40AApprox. 64°CLower hardness and good flexibilityWider thermal-processing window; finished-product shrinkage must still be validated in the actual formulation

Melting peak is not the only factor determining finished-product shrinkage. EVA ratio, crosslinking system, expansion ratio and secondary-processing conditions all affect the final result. This page uses a comparative formulation test at 70°C for 40 minutes for practical validation.

Advantages

Product Advantages

Lower Hardness

In the same 60/40 PHR comparative formulation, IUS-4065 foam reaches Asker C 35 for a softer step-in and cushioning feel.

Wider Secondary-Processing Window

A DSC melting peak of approximately 64°C helps reduce premature softening and structural relaxation during lamination, baking or hot pressing.

Significantly Lower Thermal Shrinkage

Thermal shrinkage is 0.92% after 40 minutes at 70°C, approximately 71–74% lower than the DF610 and ENGAGE 8842 comparative formulations.

Improved Elongation

Elongation at break reaches 252.36%, approximately 9–11% higher than the two comparative formulations, demonstrating good flexibility.

Rebound Maintained

Even with substantially lower hardness, ball rebound remains at 60%, balancing softness and elasticity.

Formulation and Production Support

Starting formulations, samples, physical-property testing and production validation can be provided according to target hardness, expansion ratio, density and dimensional-shrinkage requirements.

Product Description

Designed for EVA and POE Foam Systems

IUS-4065 is a high-performance elastomer modifier with a material hardness of approximately Shore A 40 and a DSC melting peak of approximately 64°C. A suitable EVA/POE ratio, crosslinking system and foaming conditions can improve dimensional retention after secondary processing.

It is not a general-purpose TPE focused only on low hardness; it is designed to address the development challenge of balancing softness, rebound and dimensional stability.

Comparison of heat deformation in low-melting materials and dimensional stability in IUS-4065  
Low-melting material heat deformation versus IUS-4065 dimensional stability
Internal Validation

Internal Performance Validation

EVA 7470M/comparison material = 60/40 PHR; expansion ratio 160%. Data are typical values under the specified formulation and conditions.

IUS-4065 foamed-product hardness comparison chart
IUS-4065 hardness is 35C, approximately 15–17% lower than the two comparative formulations.
IUS-4065 thermal-shrinkage comparison chart
Thermal shrinkage is 0.92%, approximately 71–74% lower than the two comparative formulations.
EVA foam thermal shrinkage comparison of IUS-4065, DF610 and ENGAGE 8842 at 70°C  
EVA 7470M/comparison material = 60/40 PHR; expansion ratio 160%; lower values are better.

Soft Does Not Have to Mean Shrink-Prone — IUS-4065 Balances Flexibility and Heat-Resistant Dimensional Stability

After testing at 70°C for 60 minutes, IUS-4065 shows only 1.38% thermal shrinkage and excellent heat-resistant dimensional stability. Request a sample to validate your formulation and processing conditions.

Complete Property Comparison

Test itemUnit and conditionDF610ENGAGE 8842IUS-4065Interpretation
HardnessAsker C414235Softer
Specific gravityg/cm³0.18260.18750.1816Lowest
Tensile strengthkgf/cm²19.7319.0518.25Slightly lower but comparable
Elongation at break%227.65231.43252.36Highest
Tear strengthkgf/cm8.568.087.46Optimize to requirements
Compression set% 23°C 6h28.5029.1231.67Slightly higher
Thermal shrinkage% 70°C 40min3.603.200.92Significantly lower
Ball rebound%606160Maintained
Expansion ratio%160160160Same

IUS-4065 provides lower hardness, higher elongation and substantially reduced thermal shrinkage. Tensile and tear strength are slightly lower and compression set is slightly higher, so the formulation should be optimized for actual product requirements.

Characteristics

Product Characteristics

ItemTypical IUS-4065 Data
Product typeUltra-soft, low-shrink elastomer modifier
Material appearanceTranslucent white pellets
Material hardnessApprox. Shore A 40
DSC melting peakApprox. 64°C
Primary compatible systemsEVA/POE and elastomer foam formulations
Core functionSoftening, rebound retention and improved dimensional stability after secondary processing
Applicable processesChemical foaming, injection foaming, compression molding, cold/hot pressing and lamination
Formulation approachAdjust addition ratio according to target hardness, expansion ratio, mechanical properties and processing conditions

Main Application Areas

Ultra-soft EVA/POE foam midsoles

High-rebound athletic midsoles

Functional insoles and foot-care products

Cushioning, shock-absorption and energy-return components

Sports-protection and flexible-support materials

Cold/hot-pressed and secondary-laminated foam products

Main Application Areas

From Formulation Selection to Production Validation

Provide the curent material grade, formulation ratio, target hardness, expansion ratio and secondary-processing conditions so we canevaluate a starting formulation, trial samples, mechanical properties and secondary thermal shrinkage.

The data on this page are internal typical values under specified formulation and test conditions. They are for material screening and formulation-development reference only and do not constitute guaranteed specifications for every formulation, process or finished product.

Request a sample to validate your formulation and processing conditions
From Formulation Selection to Production Validation

Other Products

Explore more material grades and applications

View More Products
READY TO BUILD WHAT'S NEXT?

Start your next product
with a better material.

Share your project requirements and contact details. A materials engineer will respond within 24 hours with recommendations and sample options.

24h Engineer Response